Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 11.5 J @Tempering Temp. 551.7 °C |
8.50 ft-lb @Tempering Temp. 1025 °F |
hardened at 2200°F, then tempered; C-notch |
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |