Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Stiffness | 65.00 MPa | 9427 psi | ASTM D747 |
Lubrizol ESTANE® 58156 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |