Flexural Stiffness 430.00 MPa
62366 psi
ASTM D747
Lubrizol ESTANE® X1013 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..