Flexural Stiffness 217.4 MPa

@Temperature 23.0 °C
31530 psi

@Temperature 73.4 °F
ASTM D747
Lubrizol Estane® 58144 Thermoplastic Polyurethane
Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer..