Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 12.6 J | >= 9.30 ft-lb | ASTM D5420 |
S&E Specialty Polymers GPP6100-116C PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |