Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 11.5 J | 8.50 ft-lb | ASTM D5420 |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |