Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 7.909 J | 5.833 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 3014 XUGW Polypropylene Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase |