RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 7.12 J
5.25 ft-lb
ASTM D5420
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.