Mechanical Properties Metric English Comments
Gardner Impact >= 67.8 J
>= 50.0 ft-lb
ASTM D5420
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled
Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro..