Mechanical Properties Metric English Comments
Gardner Impact 6.10 J
4.50 ft-lb
ASTM D3029
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..