Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 7.90 J | 5.83 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 4002 C BLK 40% Filler Content Polypropylene This product is a high impact PP copolymer developed for extrusion applications. The product lends itself well for automation of nail-gun operation, requiring good melt strength and impact resistan.. |