Polymer Property : Gardner Impact = 5.197 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 5.197 J
3.833 ft-lb
ASTM D3029
Plastics Group Polifil® RMT-20 20% Talc-Reinforced Polypropylene, High Impact
Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis..
Gardner Impact 5.197 J
3.833 ft-lb
ASTM D3029
Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the abili..