Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.26422 - 40.6746 J @Temperature -30.0 - -20.0 °C |
1.67000 - 30.0000 ft-lb @Temperature -22.0 - -4.00 °F |
Average value: 23.4 J Grade Count:21 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |