Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Gardner Impact | 48.0 J @Temperature -30.0 °C |
35.4 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |