Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 3.70 J | 2.73 ft-lb | reported as J/cm; ASTM D3029-GB, unpainted |
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |