Mechanical Properties Metric English Comments
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
Gardner Impact 3.60 J
2.66 ft-lb
ASTM D5420
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.