Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 4.07 J | 3.00 ft-lb | ASTM D5420 |
RheTech Products M12P250-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Filler panelsHVAC ductsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 4.07 J | 3.00 ft-lb | ASTM D5420 |
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |