Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 260 J @Thickness 3.17 mm |
>= 192 ft-lb @Thickness 0.125 in |
ASTM D5420 |
S&E Specialty Polymers GPP™ 1005M-EXLT PP Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |