Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 35.70 J | 26.33 ft-lb | ASTM D3029 |
Multibase Nylex™ 1404 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |