Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 25.3 J @Temperature 23.0 °C |
18.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 62 mil |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Gardner Impact | 25.3 J @Temperature 23.0 °C |
18.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 62 mil |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |