Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 23.3 J @Thickness 3.17 mm, Temperature -30.0 °C |
17.2 ft-lb @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D5420 |
ExxonMobil PP7035E5 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |