Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 31.1 J | 22.9 ft-lb | ASTM D5420-93 |
Multibase Multi-ABS 3365 High Impact ABS Data provided by Multibase. |
|||
Gardner Impact | >= 31.1 J @Thickness 3.18 mm |
>= 22.9 ft-lb @Thickness 0.125 in |
ASTM D3029 |
Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU) Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, .. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Gardner Impact | >= 31.1 J | >= 22.9 ft-lb | reverse |
Master Bond UV15SP-1 Low Viscosity, UV Curable System Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea.. |
|||
Gardner Impact | 31.0 J | 22.9 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |