Mechanical Properties Metric English Comments
Gardner Impact 2.60 J
1.92 ft-lb
Falling Weight; ASTM D3029GB
Plaskolite Optix® CA-945 Clear Impact Modified Acrylic Resin
Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times ..
Gardner Impact 2.60 J
1.92 ft-lb
Falling Weight; ASTM D3029GB
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin
Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times ..