Polymer Property : Gardner Impact = 2.22 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 3.01 J

@Temperature -30.0 °C
2.22 ft-lb

@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer
Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi..