Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D5420
RheTech Products P601-01 Polypropylene Copolymer, Black
Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D3029
M. Holland Company CP510 Polypropylene Copolymer