Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 18.08 J | 13.33 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 5012 C Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase |