Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 17.2 J @Temperature 23.0 °C |
12.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |