Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information ..
Copyright © lookpolymers.com All Rights Reserved