Mechanical Properties Metric English Comments
Gardner Impact 16.0 J
11.8 ft-lb
ASTM D5420
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Gardner Impact 16.0 J
11.8 ft-lb
Protective Coating PC-11® White Epoxy Paste
PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC..
Gardner Impact 16.0 J

@Temperature -30.0 °C
11.8 ft-lb

@Temperature -22.0 °F
ASTM D5420
Flint Hills P6C6B-134 General Purpose Impact Copolymer Polypropylene
Features: Good processability, nucleated with Antistat. Product does not contain animal derived components.Applications: Injection molding - lawn and garden partsInformation provided by Flint Hill..