Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.9 J | 15.4 ft-lb | ASTM D5420 |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.9 J | 15.4 ft-lb | ASTM D5420 |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.9 J | 15.4 ft-lb | ASTM D5420 |
Multibase Multi-Flex® TPO D 5305 Multi-Flex® D 5303 is a TOP compound for automotive applications such as bumper covers and side panels.Data provided by Multibase. |
|||
Gardner Impact | 20.9 J | 15.4 ft-lb | ASTM D5420 |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |