Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 3.62004 - 19.4334 J @Temperature -30.0 - -5.56 °C |
2.67000 - 14.3334 ft-lb @Temperature -22.0 - 22.0 °F |
Average value: 8.81 J Grade Count:4 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |