Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 14.1 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 14.1 J
10.4 ft-lb
ASTM D5420
PolyOne OnForce™ LFT NY-50LGF/001 HS Natural Polyamide 6 (Nylon 6)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Gardner Impact 14.1 J
10.4 ft-lb
ASTM D3029
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Gardner Impact 14.1 J
10.4 ft-lb
ASTM D3029
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Gardner Impact 14.1 J
10.4 ft-lb
ASTM D3029
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Gardner Impact 14.1 - 22.6 J
10.4 - 16.7 ft-lb
Average value: 17.7 J Grade Count:12
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Gardner Impact >= 14.1 J
>= 10.4 ft-lb
ASTM D3029
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact >= 14.1 J
>= 10.4 ft-lb
ASTM D3029
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact >= 14.1 J
>= 10.4 ft-lb
ASTM D3029
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.