Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 13.1 J | 9.66 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT AM-60LGF/001 Natural Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 13.1 J | 9.66 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |