Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 10.17 J | 7.500 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Gardner Impact | 10.17 J | 7.500 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Gardner Impact | 10.17 J | 7.500 ft-lb | ASTM D3029 |
Multibase Nylex™ 2185 R20 Natural Polyamide + PP Forms: PelletsInformation provided by Multibase |