Mechanical Properties Metric English Comments
Gardner Impact 1.695 J
1.250 ft-lb
ASTM D3029
Multibase Multi-Pro® 1508 M Polypropylene
Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase