Polymer Property : Gardner Impact = 1.47 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 2.00 J

@Temperature -30.0 °C
1.47 ft-lb

@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer
Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil..