Polymer Property : Gardner Impact = 1.17 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 1.59 J
1.17 ft-lb
ASTM D5420
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade
Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 1.58 J

@Thickness 3.17 mm
1.17 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Gardner Impact 1.58 J

@Thickness 3.17 mm
1.17 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Gardner Impact 1.59 J
1.17 ft-lb
ASTM D5420
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 1.58 - 11.0 J
1.17 - 8.11 ft-lb
Average value: 4.61 J Grade Count:47
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..