Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.24 J | 0.917 ft-lb | ASTM D3029 |
Plastics Group Polifil® C-30 30% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Gardner Impact | 1.24 - 40.7 J | 0.917 - 30.0 ft-lb | Average value: 14.2 J Grade Count:18 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |