Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 0.583 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black
Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products G13P100-01 13% Glass Fiber Reinforced Polypropylene, Black
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural
Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural
Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black
Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.790 J
0.583 ft-lb
ASTM D5420
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey
Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved