Mechanical Properties Metric English Comments
Gardner Impact 0.498 J
0.367 ft-lb
ASTM D5420
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.