Mechanical Properties Metric English Comments
Gardner Impact 0.294 J

@Temperature 23.0 °C
0.217 ft-lb

@Temperature 73.4 °F
per mil, 1/2" R Tup
Axiall HH-2000 Rigid PVC, Molding
Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent ..