Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.285 J | 0.210 ft-lb | per mil; ASTM D-4226 |
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |