Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact | <= 1.00 J | <= 0.738 ft-lb | |
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |