Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 1363 kJ/m² @Temperature 23.0 °C |
648.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; Long specimen; ASTM D1822 |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |