Polymer Property : Tensile Impact Strength = 325 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 683 kJ/m²

@Temperature -20.0 °C
325 ft-lb/in²

@Temperature -4.00 °F
ASTM D1822
Diamond Polymers NPP10-2528 Ethylene Vinyl Acetate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.