Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 2.00 J/cm @Thickness 5.00 mm, Temperature -40.0 °C |
0.00375 ft-lb/mil @Thickness 0.197 in, Temperature -40.0 °F |
ARM Method |
SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cyc.. |
|||
Dart Drop Total Energy | 2.00 J/cm @Thickness 5.00 mm, Temperature -40.0 °C |
0.00375 ft-lb/mil @Thickness 0.197 in, Temperature -40.0 °F |
ARM Method |
SCG Chemicals EL-Leneâ„¢ M735 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle.. |