Mechanical Properties Metric English Comments
Dart Drop Total Energy 570 J/cm
1.07 ft-lb/mil
Puncture Resistance; SABIC Method
SABIC 318B Linear Low Density Polyethylene for Cast Film
Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Dart Drop Total Energy 570 - 890 J/cm
1.07 - 1.67 ft-lb/mil
Average value: 656 J/cm Grade Count:7
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..