Polymer Property : Dart Drop Total Energy = 0.169 ft-lb/mil
Polymer Property :
Dart Drop Total Energy =
0.169 ft-lb/mil
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Dart Drop Total Energy
90.3
J/cm
0.169
ft-lb/mil
ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne