Polymer Property : Dart Drop Total Energy = 0.0920 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 49.1 J/cm
0.0920 ft-lb/mil
23°C, C.125 Tup, Method A; ASTM D-4226
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
Dart Drop Total Energy 49.1 J/cm
0.0920 ft-lb/mil
23°C, C.125 Tup, Method A; ASTM D-4226
Axiall 8150 Rigid PVC, Extrusion & Molding
Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista..