Polymer Property : Dart Drop Total Energy = 0.00468 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin
Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf..
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ M40 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-su..
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such..
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin
Natural base resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such a..
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ S10 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as ..